Last updated:

Most metallized polyethylene is bought for light blocking and for a seal. This high-barrier grade is bought for barrier. The aluminium still blocks light, but the barrier that makes this film worth its price comes from a barrier coating on the reverse face of the web — and that coating is also the reason this film cannot be sealed at all.

If you are comparing it with our standard metallized PE, the two are separate products, not two versions of one film. The standard grade seals and blocks light. This one carries an oxygen and moisture barrier, and it seals nothing.

Oxygen and water vapor transmission

PropertyValueUnit
Oxygen transmission rate (OTR)below 1cm³/(m²·24 h)
Water vapor transmission rate (WVTR)below 1g/(m²·24 h)

Both figures sit below 1, which is low for a single metallized web with no second substrate, and this one gets there on a PE base. The whole point of the film is that trade, and it is also why it costs more than an ordinary metallized PET (VMPET) web: the performance is bought, not assumed.

One caution before those numbers go into a specification: OTR and WVTR are readings, not properties. They are only comparable when measured at the same temperature, under the same relative humidity, by the same method. How ours were measured, and at what conditions, is set out below — and the same question is worth asking of anyone else you are quoting.

Where the barrier comes from

Polyethylene is a poor barrier polymer, and metallizing alone does not change that: depositing aluminium gives a PE web light blocking and a useful improvement in moisture resistance, but it does not turn PE into an oxygen barrier.

This film solves that by construction rather than by substitution. The base remains PE, the aluminium remains the light block, and the barrier function is carried by a barrier coating. Its formulation is proprietary, and the specification we publish is the transmission performance it delivers. This construction is why the numbers above are achievable on a polyethylene web at all — and why the film behaves differently on your line from a plain metallized PE.

It does not seal, and that is structural

The coated face and the metallized face are both barrier surfaces. Neither face is a sealant, so no jaw setting will produce a seal. Nothing about that can be tuned out: the barrier is made of these surfaces.

The practical consequence fixes the film’s position in a structure: it belongs in the middle. A separate PE sealant ply does the sealing on the inside, and the barrier ply sits behind it.

This is also where a specification most often goes wrong. If a buyer takes the seal strength figure from our standard metallized PE — 8.7 N/15 mm — and applies it to this film, they are quoting a property this product does not have. The two products carry separate data sheets for that reason.

Specification

ParameterValue
Thickness40 µm
Web widthUp to 2,000 mm
BarrierOTR below 1 cm³/(m²·24 h); WVTR below 1 g/(m²·24 h)
CoatingBarrier coating on the reverse face; formulation proprietary
Light blockingYes — from the aluminium layer
Heat sealNone. Barrier surfaces only
Minimum orderOne roll of 3,700 m, where the width can be matched to a production already scheduled

Two of those lines deserve a word. The film is a single 40 µm construction rather than a gauge range, because the coating and the metallizing are qualified together at that thickness. And the minimum order is a roll rather than tonnes: if your width can be matched to a run we already have scheduled, you can trial this film with a single 3,700 m roll rather than a pallet of inventory.

The structure it belongs in

This film exists to make a genuine barrier possible inside a mono-material PE pack. Three plies, all polyethylene-based:

PlyMaterialDuty
OuterMDOPE (machine-direction oriented PE)Print surface, mechanical protection, stiffness
MiddleThis film (PE base, barrier coating)Oxygen and moisture barrier, plus light block. No seal
InnerPE sealantThe seal — your initiation temperature, your dwell, your pressure

What the pack ends up with is a barrier that competes with a metallized PET laminate, light blocking, and a base web that stays inside the polyethylene family. That is what makes the finished structure compatible with the PE stream, wherever that stream exists. Whether a given pack actually gets recycled still depends on the collection stream where it is sold: the film can make a structure recyclable-compatible, it cannot deliver that outcome. The design logic behind a mono-material structure is set out separately.

The maximum web width matters here. At 2,000 mm this film is narrower than our standard metallized PE, so a converter running wide webs should check the ply width against the finished pouch layout before designing around it.

Metallized PE against metallized PET

The comparison will be made whether we write it or not, so it is better made here, with the numbers in the open.

QuestionThis filmMetallized PET
Oxygen barrierBelow 1 cm³/(m²·24 h)Higher: a standard VMPET web is not specified below 1
Moisture barrierBelow 1 g/(m²·24 h)Ask for the VMPET figure at matching conditions; it depends on metallizing quality and pinhole density, not on the polymer alone
Seal of its ownNoNo
Polymer family of the finished packPE base web plus barrier coatingPET plus PE plus adhesive
Film costHigherLower
StiffnessLowerHigher

Read down that table and the trade is visible: this film wins on oxygen barrier and on staying inside one polymer family, and it loses on price and on stiffness. It is neither the cheap route nor the stiff route: it is bought for the barrier. If a buyer needs barrier without caring which polymers end up in the pack, metallized PET is the more economical answer, and we would rather say so than sell a premium film into a job that does not need it.

Which one, in four questions

In practice the decision collapses quickly. Answer these in order and stop at the first “no”.

#QuestionIf the answer is no
1Does the pack need a real oxygen barrier?Stop. The standard metallized PE grade costs less than this film and already seals.
2Does it need to stay a single material?Stop. Metallized PET gives you the barrier at a lower film cost.
3Can your line run a 2,000 mm web, or split the ply?Stop and talk to us before designing — this film is narrower than our standard grade.
4Can the structure carry a third ply for the seal?Stop. Without a PE sealant ply there is nothing to seal this film to.

Four questions, four honest exits. Most inquiries do not reach question four, and that is the point of writing them down: it saves both sides the round trip of quoting a film that was never going to fit.

Where a metallized PET three-ply is still the right answer

There are jobs where the three-ply metallized PET structure beats this film, and they are worth naming rather than arguing around.

  • Shelf life beyond what the barrier supports. Where the target runs long and the product is genuinely oxygen-sensitive, the honest answer is a structure built for that shelf life — a foil-containing laminate, or a metallized PET build qualified below 1 — and the single-material argument is what the buyer gives up.
  • Retort and high-temperature fill. The temperature window belongs to the structure, not to the metal layer, and PET carries it better than PE.
  • Stiffness as a functional requirement. A pack that has to stand, present or run on a machine designed around a stiff web is not a job for a PE barrier ply.
  • Markets where the collection stream does not separate PE. If the pack will not be sorted into a PE stream where it is sold, the single-material argument buys the buyer nothing — and the cheaper structure wins on its own terms.
  • Structures that have already fixed a CPP or BOPP sealant. Once the seal is polypropylene, the pack has left the polyethylene family and the single-material case is gone; adding this film buys barrier at a premium where metallized PET buys it for less.

A mono-material pack is only an improvement where the material can actually be recovered; in a market without that stream, the environmental case is theoretical while the cost case is real.

What the recyclability claim does and does not say

Three sentences, kept deliberately narrow. The film is a polyethylene-based barrier ply. A pack built around it is designed to stay inside the PE stream rather than being downcycled or sent to energy recovery, where that stream exists. Whether a given pack is actually collected and recycled depends on the stream where it is sold, on the rest of the structure, and on rules we do not set.

So the claim is about design, not about outcome. That distinction matters commercially as well as legally: a buyer who repeats “recyclable” as a certainty is making a claim their own market may not support, and the paperwork trail runs back to whoever said it first.

How the figures were measured

Our barrier figures come from the Chinese national methods, and both of them sit in the same measurement families as the ASTM and ISO methods your own laboratory works to. Oxygen is measured by GB/T 19789, the coulometric sensor method. Water vapor is measured by GB/T 26253-2010, the infrared detector method — a standard that is a modified adoption of ISO 15106-2, so for a European buyer the moisture figure already comes from the method your own laboratory recognizes.

The test conditions recorded on our reports are 21–30 °C and 40–70 % relative humidity. A range rather than a single set-point — and it is worth being explicit about what it means, because it is the one line most easily misread on a specification sheet. Water vapor transmission rises with temperature and with humidity: a figure taken at the low end of that range — 21 °C and 40 % RH — is not directly comparable with one taken at 38 °C and 90 % RH, which is the condition most often named in European and North American specifications. The range describes the conditions our report records — it does not mean the same film will read identically at 38 °C and 90 % RH.

If your specification names 38 °C and 90 % RH, or ASTM F1249, say so with the inquiry and we will confirm what this film delivers at that condition rather than invite you to convert a number. The same applies to oxygen: ask for the test report and compare at matching conditions, or send a sample to your own laboratory and check ours against it. A barrier figure is only worth the conditions printed beside it.

Food contact

The coating is the part of this film a technical reviewer will ask about, so it is worth stating plainly rather than leaving to a footnote.

This grade is made from virgin resin and is tested under the Chinese food-contact framework for both components of the construction: GB 4806.7 for the plastic material, and GB 4806.10 for the coating. The film passes the migration tests for acetic acid, ethanol, heavy metals and aromatic amines. The second standard is the relevant one here — a coated film is not covered by the plastics standard alone, and a supplier who cites only GB 4806.7 for a coated product has not addressed the coating at all.

Two related points, because they are often confused. There is no recycled-content version of this grade — it is virgin material throughout, and no PCR claim should be made for it. Recyclability is a different question: the ply is a polyethylene-based film, and a pack built around it stays in the PE stream. It is not made from recycled material, and it is compatible with the PE recycling stream where that stream exists: both are true at once.

Where your market needs a declaration we have not named — an EU or US food-contact statement, for instance — put the requirement in the inquiry and we will confirm exactly what can be issued for this construction, rather than imply a document we cannot send.

What we need to quote

Four things: the contents and their sensitivity, the target shelf life, the ply width your machine runs, and the structure you are using today. The ply width is not a formality on this film: with a 2,000 mm ceiling it decides whether the job can run on your line, and whether the one-roll minimum applies. Send us the ply width and the contents and we will confirm the structure before you commit to artwork.

Questions buyers ask about this film

What does OTR below 1 mean, and in what unit?

It means oxygen transmission below 1 cm³/(m²·24 h) — cubic centimeters of oxygen per square meter of film per 24 hours, measured to GB/T 19789, the coulometric method. Water vapor is quoted the same way in g/(m²·24 h), measured to GB/T 26253-2010. Both are ceiling values: the figure is the upper limit, not a typical or average result.

Can this film be heat sealed?

No. Both faces are barrier surfaces — the coating on one side and the metallized layer on the other — and neither is a sealant, so no jaw setting will produce a seal. The seal has to come from a separate PE ply on the inside, which is why this film sits at the middle of a three-ply structure rather than at the inner face.

Is it approved for food contact?

It is made from virgin resin and tested under the Chinese food-contact framework: GB 4806.7 for the plastic material and GB 4806.10 for the coating, and it passes the migration tests for acetic acid, ethanol, heavy metals and aromatic amines. For markets needing an EU or US declaration, put the requirement in the inquiry and we will confirm what can be issued for this construction.

Is there a recycled-content version?

No. This grade is virgin material throughout, and no PCR claim should be made for it. That is separate from recyclability: the ply is a polyethylene-based film and a pack built around it stays in the PE stream, but the film is not made from post-consumer material.

What is the minimum order?

One roll of 3,700 m, where the width can be matched to a production already scheduled. Because the film is a single 40 µm construction metallized up to 2,000 mm wide, the width is the deciding factor rather than the quantity, so send the ply width with the inquiry and we will confirm whether the one-roll minimum applies.

Why does it cost more than metallized PET?

Because the barrier is higher. An ordinary metallized PET web is normally not specified below 1 for oxygen, and metallized PET cannot be used to build a single-material pack. The extra cost buys performance and a structure option, not a brand name — and where a buyer does not need either, we recommend metallized PET instead.