Last updated:

“PE metallized film” is not one product, and treating it as one is how specifications go wrong. We make two, and they are not interchangeable: one blocks light and seals, the other carries a real barrier and does not seal at all. The difference decides which layer of your structure it can occupy, and getting it backwards costs you either the shelf life or the seal.

The standard grade: light block and seal, not oxygen barrier

Polyethylene is a poor barrier polymer. We do not work around that fact — it is the reason PE is never the oxygen-barrier layer in a structure, and why the oxygen transmission of a plain PE film is not a figure anyone quotes.

Metallizing changes part of that picture. Depositing aluminium onto a PE web gives it two things: it blocks light, and it improves moisture resistance to a measurable degree — a water vapor transmission rate (WVTR) of 2.1 g/(m²·24 h), measured on a 40 µm film. Oxygen barrier is not a performance we offer on this grade, and we would rather say so than let a specification sheet imply otherwise.

So the standard film is specified for what it actually does: it is an inner sealing web that also blocks light and takes the edge off moisture ingress. In a pack where the barrier requirement is light protection plus ordinary moisture resistance, that is often the whole job. The full specification for the standard film is on its own page.

The high-barrier grade: the barrier comes from a coating

The second product is a different construction. Its barrier does not come from the base polymer, which is still PE, and it does not come from the aluminium alone. It comes from an additional coating, and the result is a film whose oxygen transmission falls below 1 cm³/(m²·24 h) and whose water vapor transmission falls below 1 g/(m²·24 h) — with the aluminium layer supplying light blocking on top. It is supplied at 40 µm, in widths up to 2,000 mm.

The barrier sits in the coating rather than in the metal alone, which is what lets this grade read below 1 on both numbers while it stays on a PE base. The same coating is also the reason the film costs more than an ordinary metallized PET (VMPET) web: the performance is bought rather than assumed.

What it does not have is a seal. The coating and the metallized surface are barrier surfaces; neither face is a sealant. The missing seal is what puts the film in the middle of a structure, with a separate PE sealant doing the sealing on the inside. The high-barrier grade’s specification is on its own page.

Structure one: one ply fewer

The standard grade’s home is the inside of a two-ply structure. Take a three-ply build — outer print web, a light-blocking ply, inner sealant — and the standard film absorbs the light-blocking duty into the ply that was already sealing. Two plies instead of three.

What leaves the structure is a film, a lamination pass, the adhesive that the pass consumes, the energy behind it, and one fewer component to specify, stock and trace. The barrier you keep is light and moderate moisture. The barrier you give up is oxygen, and if the pack needed it, this structure was never the right answer.

Structure two: an all-PE three-ply, with the high-barrier grade in the middle

Here the second product earns its price. Three plies, all in the polyethylene family:

PlyMaterialDuty
OuterMDOPE (machine-direction oriented PE)Print surface, mechanical protection, stiffness
MiddleHigh-barrier PE metallized filmMoisture and oxygen barrier, plus light block — no seal
InnerPE sealantThe seal: your initiation temperature, your dwell, your contamination

The pack keeps a genuine barrier, keeps light blocking, and keeps its base web inside the polyethylene family — which is what makes a finished structure compatible with the PE stream wherever that stream exists. Whether a given pack is actually recycled still depends on the collection stream where it is sold; the film can make a structure recyclable-compatible, it cannot deliver that outcome. The design logic behind a mono-material structure is set out on its own page.

Note what changed: in this structure the barrier ply is the one that cannot seal, and the sealing is done by a third ply. In structure one the barrier ply is the seal. Two products, two architectures — they are not two settings of the same film.

Choosing between them

Your requirementAnswerBecause
Light protection, ordinary moisture, seal neededStandard grade, inner webThat is exactly its job, at a lower cost than the high-barrier grade
Oxygen barrier requiredHigh-barrier gradeThe standard grade does not offer it
Oxygen barrier and single-material packHigh-barrier grade, middle ply, plus PE sealantThe combination that delivers both
Barrier only, no interest in single materialMetallized PETCosts less per square meter than the high-barrier grade, with oxygen transmission specified no lower than 1 cm³/(m²·24 h)

Reading the numbers correctly

The seal strength figure on our standard specification — 8.7 N/15 mm, upper jaw 120 °C, lower jaw 80 °C, 1.0 s dwell, 0.2 MPa — belongs to the standard grade’s sealant face. It does not apply to the high-barrier grade, because that film does not seal at all.

The barrier figures come with their own method: oxygen by GB/T 19789, the coulometric method, and water vapor by GB/T 26253-2010, the infrared method — a modified adoption of ISO 15106-2 — at 21–30 °C and 40–70 % relative humidity. A figure quoted at 38 °C and 90 % RH is a different measurement of the same film, not a better one.

Likewise the WVTR figure of 2.1 g/(m²·24 h) describes the standard grade. The high-barrier grade is below 1 g/(m²·24 h), and below 1 cm³/(m²·24 h) for oxygen. Quoting one where the other belongs is the error we see most often in incoming specifications, and it usually surfaces at the filling line rather than in the quote.

Cost, and one route we do not recommend

The standard grade costs less than the high-barrier grade, and the high-barrier grade costs more than an ordinary metallized PET — the barrier is genuinely higher, and that is what the money buys. Whether the structure lands cheaper overall is a calculation about which plies you remove, not a comparison of film prices. Send us the structure you run today and we will work through it rather than claim a percentage we cannot stand behind.

One combination we talk buyers out of: laminating the standard grade to cast polypropylene (CPP). CPP would be the sealant, which leaves the standard film doing light blocking and moderate moisture only — and that duty is bought more cheaply as metallized PET. The pairing also leaves the polyethylene family, so it loses the single-material argument, and the standard grade laminated to CPP is less stiff than the metallized PET and CPP equivalent. If your structure calls for CPP as the sealant, the barrier web should be metallized PET.

Getting to a trial

Both grades run on our own metallizing lines, but not to the same dimensions, and it is worth checking before you design around an assumption. The standard grade is made in 40, 60, 70 and 80 µm, in widths of 3,000–3,200 mm. The high-barrier grade is a single 40 µm construction, metallized in widths up to 2,000 mm, with a minimum order of one roll of 3,700 m where the width can be matched to a production already scheduled. Samples of either grade are ready in 15–20 days.

Because the metallizing and the converting steps are in-house, a trial roll can be checked against your converting window before a production order exists. Printing, lamination and bag-making can be trialled on the same site as the film, which removes the usual loop of the film supplier and the converter each pointing at the other.

What we need to specify a structure

Five things: the contents and their sensitivity, the target shelf life, whether the pack must be a single material, the structure you run today, and the machine and print method. From those we will confirm which grade your structure needs, which ply it replaces, and what the conversion trial should look like. Send us the five things and we will come back with a structure rather than a catalog.

Questions buyers ask about the two grades

Which of the two PE metallized films should I use?

Start with the failure mode. If the pack needs oxygen protection, it is the high-barrier grade; the standard grade does not offer oxygen barrier at all. If the requirement is light protection plus ordinary moisture and the ply has to seal, it is the standard grade, and it costs less than the high-barrier grade. The two are separate products, not two settings of one film.

Can I use the standard grade where I need an oxygen barrier?

No. Metallizing a PE web gives it light blocking and a useful improvement in moisture resistance, but polyethylene remains a poor oxygen barrier and the standard grade does not claim one. Specifying it into an oxygen-sensitive pack is how a shelf-life claim fails after the artwork is approved.

Why can the high-barrier grade not be used as the inner ply?

Because it has no sealant surface. Both faces are barrier surfaces, and neither will produce a seal at any jaw setting. That is structural rather than a matter of settings, which is why the film belongs at the middle ply with a PE sealant inside it.

Is a two-ply structure recyclable?

The standard grade is a polyethylene-based film — a PE web with a thin aluminium layer — so a two-ply built around it stays in the PE family and is compatible with PE recycling streams. Whether a finished pack is actually collected and recycled depends on the stream where it is sold and on the rest of the structure, which is why we describe the structure as recyclable-compatible rather than recyclable.

Can I mix the two grades in one order?

Yes, and the MOQs differ, so it is worth planning them together: the standard grade starts at 1,000 kg in the four standard gauges, while the high-barrier grade starts at one roll of 3,700 m where the width matches a scheduled production. Tell us both requirements in one inquiry and we will quote them against the same delivery.